  • • PROPERTIES OF LIQUID RESIN :
    Viscosity, 25°C, Poises...............................4~6
    Specific Gravity...............................1.11~1.13
    Gel Time, Minutes, 25°C...............................8~15
    Thixotropy Index, 25°C...............................1.5~2.5

 

  • • CURING CONDITION :
    Red Accelerator,Co-oct(Co6%).....................0.5%
    Hardener, MEKPO (PO contents, 55%).....................1.0%


  • • PROPERTIES OF CURED RESIN:
     Contents 30% of fiberglass matUnfilled Casting
    (No. 450 3-plies) 
    Flexural Strength, kg/mm220.4N/A
    Flexural Modulus, kg/mm2880N/A
    Tensile Strength, kg/mm212.4N/A
    Hardness, Barcol 934-1N/A42

 

* The specimens cured at room temperature + two-hour postcure at 80°C